Cathodic Disbondment Test

A 4" by 4" plate from each sample is used to test the coating for resistance to disbonding under electrical stress at elevated temperature. A 3 percent NaCl solution and a potential of 3.5 DC volts (reference calomel electrode) is impressed through a 3 millimeter drilled holiday. Electrolyte solution temperature is maintained at 150 degrees Fahrenheit for 24 hours. After the test period, radial cuts are made through the coating at a point 45 degrees from the edge of the holiday. The radius of disbondment is measured by inserting the knife point under the coating to "flick" the coating until a definite resistance to this levering action can be noted.


PreviousNext


-----

Bayou Coating LLC
A Subsidiary of Stupp Bros., Inc.


Copyright © 1997 Bayou Coating LLC
Houston Sales Office
650 N. Sam Houston Parkway East
Houston, TX 77060   USA

Phone: 281.591.1614
Fax: 281.591.0284
E-mail

-----

ISO 9002 INGAA NACE NAPCA
About Us Plant Tour Products/Services Portfolio Estimates What's New Home